Case Study: 15-Year Color Retention of CICP Pigments in PVC Window Profiles

Quick answerProfiles coloured with SOLCRY BROWN 3201 (P.Br 33 zinc iron chromite brown spinel, CAS 68186-88-9) at 1.5% loading in Ca/Zn-stabilised rigid PVC averaged ΔE*ab 1.2 after fifteen years of exterior exposure - below the roughly 1.5 difference at which the eye begins to notice a colour change.

Why a window profile is a hard test for any pigment

A window profile lives outdoors for two decades and is expected to look new at the end of it. In service it sees direct sunlight, temperature cycling from about -20 °C to +60 °C, rain, frost and urban pollutants, and it does so while carrying a heat history from extrusion that has already stressed the PVC compound once. The pigment has to survive all of that without moving, fading or migrating into the surface.

Browns and dark greys are the hardest shades to hold. They sit at the low-reflectance end of the palette, where a small absolute change in pigment chemistry shows up as a visible shift, and they absorb more solar energy than white profiles, so the surface runs hotter. A brown profile that stays inside ΔE*ab 1.5 for fifteen years is therefore a strong statement about the pigment's stability.

The trial: 1.5% BROWN 3201 in Ca/Zn rigid PVC

The study followed profiles from three European production lines running Ca/Zn-stabilised rigid PVC coloured with BROWN 3201 at 1.5% loading. Samples were measured annually with a spectrophotometer under the same illumination and observer conditions, and the colour difference was recorded against the original production reference rather than against a refreshed master.

That last detail matters. Comparing a weathered sample with a freshly moulded plaque overstates change, because the reference itself may have shifted. Comparing against the original lot keeps the measurement honest, and it is the method used for the figures reported here. The same panels were inspected visually each year for chalking, cracking and surface erosion.

Results after fifteen years

After fifteen years the average ΔE*ab was 1.2. For context, 1.5 is about the point at which a trained eye notices a side-by-side difference, so the profiles stayed inside the threshold that matters commercially: no customer complaint, no reclamation, no repaint. The spread across the three lines was small enough to be explained by exposure orientation rather than by pigment variability.

No chalking, cracking or surface degradation was observed on any of the panels. That is the second half of the result. A pigment can hold its colour while the polymer around it fails, and a profile that has gone chalky or micro-cracked has failed even if the measured colour is unchanged. Here the polymer and the pigment both held.

Why the spinel lattice holds the shade

BROWN 3201 is a zinc iron chromite brown spinel. Its colour comes from iron and chromium held inside a cubic close-packed oxide lattice, not from an organic chromophore that can be attacked by UV or oxidized by air. The chromophore is part of the crystal, so there is no dye to migrate, no double bond to break and no volatile fragment to lose. That is why the shade survives fifteen years of UV without a fade mechanism to drive it.

The same lattice explains the chemical side of the performance. CICP pigments hold from pH 1 to pH 14, and they are tested to 800 °C by CF-33 with ΔE*ab at or below 3.0. Light fastness is grade 8 on the blue wool scale and weathering is rated at 30+ years, supported by 5000 h of xenon-arc exposure. For a profile extruder, those are the numbers that turn a fifteen-year warranty into an engineering calculation.

What a profile extruder should specify

Name the C.I. pigment and the CAS number in the specification, not just the shade. For a brown PVC profile that means P.Br 33 at CAS 68186-88-9, with the crystal form stated as spinel. Require a batch certificate of analysis that reports the C.I. identity, the heat resistance result by CF-33 and the light fastness grade, and ask for xenon-arc weathering data on the pigment rather than only on the finished profile.

Finally, ask how the pigment behaves in the compound. Co-extrusion is unforgiving of anything that disturbs the melt, and a pigment that changes the semicrystalline morphology of PVC will show up as warpage long before it shows up as a colour problem. A grade that has been run for fifteen years in three production lines has already answered that question.