SOLCRY®
Home / Applications / Plastics and Polymer Masterbatch

CICP Pigments for Plastics and Polymer Masterbatch

Quick answerPlastics put a pigment through a melt, a shear field and a cooling cycle before the part even exists. CICP pigments survive all three: 800 °C heat resistance covers any polymer melt, the spinel grades are processing-neutral in PVC, and the dense oxide particles can be dispersed to full colour development with the right masterbatch formulation.

The heat history is not the problem

Engineering resins process between roughly 200 °C and 350 °C. With heat resistance of 800 °C by CF-33, a CICP pigment is not the component that limits the processing window, which means the formulation can be optimized around the polymer and the stabilizer package instead of around the colourant.

That matters most in polymers that are already running near their thermal limit. A pigment that begins to degrade at the melt temperature produces colour drift, odour and plate-out; a calcined oxide has nothing left to decompose.

PVC profiles: processing neutrality

PVC is the application where the pigment has to be more than inert. In a co-extruded window profile, the cap layer is thin, the pigment loading is high and the profile has to come out straight. Anisotropic pigment particles can disturb the semicrystalline morphology of PVC and produce differential shrinkage, which shows up as warpage after cooling.

Zinc iron chromite brown spinel (P.Br 33, CAS 68186-88-9) has been used in production for long enough that its behaviour is characterized: equiaxed spinel particles, zero warpage, and compatibility with tin, Ca/Zn and organic stabilizer systems. Fifteen-year colour retention data from installed profiles confirms ΔE*ab below 1.5.

Masterbatch: dense pigment, different rules

CICP pigments have a specific gravity of roughly 4.0–5.5 g/cm³, far above organic pigments, and that changes the masterbatch problem. Feeding, wetting and screw configuration matter more than raw pigment loading. The recommended approach uses a 40:1 L/D co-rotating twin-screw extruder with distributive elements in the first third, dispersive kneading blocks in the middle and gentle conveying at the end.

Dispersant selection is equally important. For CICP blacks in polyolefins, polyethylene wax at 2–4% on pigment provides the wetting needed, and over-dispersion can actually reduce colour strength by breaking crystallites below their optimal scattering size. A systematic approach reaches 95%+ colour development.

Grade selection for plastics

Frequently asked questions

Can CICP pigments be used in engineering plastics?

Yes. Heat resistance of 800 °C by CF-33 covers every engineering resin melt temperature, so the pigment is not the limiting component of the formulation.

Why is CICP black harder to disperse than organic black?

Because of density. CICP pigments have a specific gravity of 4.0–5.5 g/cm³, so feeding and wetting matter more than loading. A 40:1 L/D twin-screw with the right kneading block placement and 2–4% polyethylene wax on pigment reaches full development.

Which grade is used for PVC window profiles?

Zinc iron chromite brown spinel, P.Br 33 at CAS 68186-88-9 (BR3201). It shows zero warpage in co-extrusion and is compatible with tin, Ca/Zn and organic stabilizers.